INTELLIGENT WORK FORUMS
FOR ENGINEERING PROFESSIONALS

Log In

Come Join Us!

Are you an
Engineering professional?
Join Eng-Tips Forums!
  • Talk With Other Members
  • Be Notified Of Responses
    To Your Posts
  • Keyword Search
  • One-Click Access To Your
    Favorite Forums
  • Automated Signatures
    On Your Posts
  • Best Of All, It's Free!
  • Students Click Here

*Eng-Tips's functionality depends on members receiving e-mail. By joining you are opting in to receive e-mail.

Posting Guidelines

Promoting, selling, recruiting, coursework and thesis posting is forbidden.

Students Click Here

Jobs

UCS-85C

UCS-85C

(OP)
What is your understanding of UCS – 85(c)

RE: UCS-85C

Here is UCS-85 (c)

(c) The material used in the vessel shall be represented
by test specimens which have been subjected to the same
heat treatments above the lower transformation temperature
and postweld heat treatment
except as provided in
(e), (f), (g), (h), and (i) below. The kind and number of
tests and test results shall be as required by the material
specification.
The vessel Manufacturer shall specify the
temperature, time, and cooling rates to which the material
will be subjected during fabrication, except as permitted
in (h) below. Material from which the specimens are prepared
shall be heated at the specified temperature within
reasonable tolerances such as are normal in actual fabrication
.
The total time at temperature shall be at least 80% of
the total time at temperature during actual heat treatment
of the product and may be performed in a single cycle.

What don't you understand? I underlined important points to review. The concern is to validate by testing the properties of the steel subjected to re-heat treatment after forming or welding.

Red Flag This Post

Please let us know here why this post is inappropriate. Reasons such as off-topic, duplicates, flames, illegal, vulgar, or students posting their homework.

Red Flag Submitted

Thank you for helping keep Eng-Tips Forums free from inappropriate posts.
The Eng-Tips staff will check this out and take appropriate action.