Stellite 6 on Stellite 6 galling?
Stellite 6 on Stellite 6 galling?
(OP)
Is anybody have experience with galling issues in ball valves with ball and seats being hardfaced with Stellite 6?
In my case the valve is 8" CL300, op. temp -9/+65 Deg C. op. pressure limit is 48 Barg.
In my case the valve is 8" CL300, op. temp -9/+65 Deg C. op. pressure limit is 48 Barg.