thread723-211593: Magnetic properties of SS 416 (B-H)
Great post! You say that you downloaded this data (see below). Where did you download it from?
Report
dgallup (Automotive)7 Mar 08 11:37
I have this data that I downloaded when I tried using FEMM.
I make no claims to it's accuracy.
B (T) H (A/m)
0.000 0.0
0.200 318.3
0.426 477.5
0.761 795.8
1.097 1591.6
1.233 2387.3
1.335 3978.9
1.460 7957.8
1.590 15915.5
1.690 31831.0
1.724 44456.3
1.740 55704.3
Great post! You say that you downloaded this data (see below). Where did you download it from?
Report
dgallup (Automotive)7 Mar 08 11:37
I have this data that I downloaded when I tried using FEMM.
I make no claims to it's accuracy.
B (T) H (A/m)
0.000 0.0
0.200 318.3
0.426 477.5
0.761 795.8
1.097 1591.6
1.233 2387.3
1.335 3978.9
1.460 7957.8
1.590 15915.5
1.690 31831.0
1.724 44456.3
1.740 55704.3