Hi,
we are facing a pump seal leak problem, Pump seal have elastomer rings by KSB germany for our deethanizer reflux pumps, we used Mobil Jet Oil II as barrier fluid instead of vendor recommended barrier fluid ''Klüberfluid NH1 4-005'' Mobil jet two have same properties as vendor recommended one.
I'm curious to know about mobil jet oil II may be getting diluted with propane and butane and losing its properties and damaging the elastomer rings.
Can any one explain bit on this issue/
Thanks
10815L
we are facing a pump seal leak problem, Pump seal have elastomer rings by KSB germany for our deethanizer reflux pumps, we used Mobil Jet Oil II as barrier fluid instead of vendor recommended barrier fluid ''Klüberfluid NH1 4-005'' Mobil jet two have same properties as vendor recommended one.
I'm curious to know about mobil jet oil II may be getting diluted with propane and butane and losing its properties and damaging the elastomer rings.
Can any one explain bit on this issue/
Thanks
10815L





RE: Deethanizer Reflux pump Seal Damage
RE: Deethanizer Reflux pump Seal Damage
RE: Deethanizer Reflux pump Seal Damage
RE: Deethanizer Reflux pump Seal Damage
Klüberfluid NH1 4-005 was recommended by vendor (eagleburman),
Thanks
RE: Deethanizer Reflux pump Seal Damage
Regards