INTELLIGENT WORK FORUMS
FOR ENGINEERING PROFESSIONALS

Log In

Come Join Us!

Are you an
Engineering professional?
Join Eng-Tips Forums!
  • Talk With Other Members
  • Be Notified Of Responses
    To Your Posts
  • Keyword Search
  • One-Click Access To Your
    Favorite Forums
  • Automated Signatures
    On Your Posts
  • Best Of All, It's Free!
  • Students Click Here

*Eng-Tips's functionality depends on members receiving e-mail. By joining you are opting in to receive e-mail.

Posting Guidelines

Promoting, selling, recruiting, coursework and thesis posting is forbidden.

Students Click Here

Jobs

AASHTO Charpy V-Notch

AASHTO Charpy V-Notch

AASHTO Charpy V-Notch

(OP)
I am putting together some drawings for structural steel and have been asked what are the Charpy V-notch requirements for this material. I see in ASTM A709 that the notch toughness requirements are to be in accordance with AASHTO. What are these requirements? I looked through LTS-4 and did not see any specific requirements. Also in A709 Table 8 there are values for Zones 1, 2 & 3. What are these zones?

RE: AASHTO Charpy V-Notch

AASHTO LRFD Bridge Design Spec Table 6.6.2-2 lists the requirements. The zone relates to the temperate zone designation, see Table 6.6.2-1. There is a nice paragraph in section 6.6 that gives some information.

Red Flag This Post

Please let us know here why this post is inappropriate. Reasons such as off-topic, duplicates, flames, illegal, vulgar, or students posting their homework.

Red Flag Submitted

Thank you for helping keep Eng-Tips Forums free from inappropriate posts.
The Eng-Tips staff will check this out and take appropriate action.

Reply To This Thread

Posting in the Eng-Tips forums is a member-only feature.

Click Here to join Eng-Tips and talk with other members!


Resources