Hi,
Does anyone have any good web links/resources for laser etching practice? Handbook for Laser Etching engineering?
I have a laser etcher that runs well with Carbon Steel but poor with Nickel and Brass (even after playing with some settings). Also will sometimes will run inconsistent.
I don't have enough experience to know what to look for. I am looking for a practical and in depth resource on the subject.
Thanks All.
Does anyone have any good web links/resources for laser etching practice? Handbook for Laser Etching engineering?
I have a laser etcher that runs well with Carbon Steel but poor with Nickel and Brass (even after playing with some settings). Also will sometimes will run inconsistent.
I don't have enough experience to know what to look for. I am looking for a practical and in depth resource on the subject.
Thanks All.