INTELLIGENT WORK FORUMS
FOR ENGINEERING PROFESSIONALS

Log In

Come Join Us!

Are you an
Engineering professional?
Join Eng-Tips Forums!
  • Talk With Other Members
  • Be Notified Of Responses
    To Your Posts
  • Keyword Search
  • One-Click Access To Your
    Favorite Forums
  • Automated Signatures
    On Your Posts
  • Best Of All, It's Free!
  • Students Click Here

*Eng-Tips's functionality depends on members receiving e-mail. By joining you are opting in to receive e-mail.

Posting Guidelines

Promoting, selling, recruiting, coursework and thesis posting is forbidden.

Students Click Here

Jobs

ASME QW-452.4 and QW-452.6

ASME QW-452.4 and QW-452.6

ASME QW-452.4 and QW-452.6

(OP)
My question is as follows:

If a welder is qualified to weld on a pipe >2.5 NPS does this qualify him/her to weld a fillet weld on a pipe <2.5 NPS?

RE: ASME QW-452.4 and QW-452.6

Did the welder qualify on a groove weld, or fillet weld?

RE: ASME QW-452.4 and QW-452.6

No, if qualified by a fillet in accordance with ASME IX, Table QW-452.4;

Yes if qualified by groove weld per ASME IX Table QW-452.6.

Red Flag This Post

Please let us know here why this post is inappropriate. Reasons such as off-topic, duplicates, flames, illegal, vulgar, or students posting their homework.

Red Flag Submitted

Thank you for helping keep Eng-Tips Forums free from inappropriate posts.
The Eng-Tips staff will check this out and take appropriate action.

Reply To This Thread

Posting in the Eng-Tips forums is a member-only feature.

Click Here to join Eng-Tips and talk with other members!


Resources