Welding of SS321 pipe with SS347
Welding of SS321 pipe with SS347
(OP)
Dear Material experts,
I have a pipe spool of SS321 being used for 1" riser along the flare stack.
I have short supply of material SS321, 1" pipe
Please suggest if I can use SS347 pipe spool available with me.
I need to weld the material as it has socket weld joints.
As per my study, E-347-16 welding rod is used for both, SS321 and SS347 material.
Please suggest if I can use SS347 pipe spool available with me.
I have a pipe spool of SS321 being used for 1" riser along the flare stack.
I have short supply of material SS321, 1" pipe
Please suggest if I can use SS347 pipe spool available with me.
I need to weld the material as it has socket weld joints.
As per my study, E-347-16 welding rod is used for both, SS321 and SS347 material.
Please suggest if I can use SS347 pipe spool available with me.





RE: Welding of SS321 pipe with SS347
RE: Welding of SS321 pipe with SS347
= = = = = = = = = = = = = = = = = = = =
P.E. Metallurgy, Plymouth Tube