INTELLIGENT WORK FORUMS
FOR ENGINEERING PROFESSIONALS

Log In

Come Join Us!

Are you an
Engineering professional?
Join Eng-Tips Forums!
  • Talk With Other Members
  • Be Notified Of Responses
    To Your Posts
  • Keyword Search
  • One-Click Access To Your
    Favorite Forums
  • Automated Signatures
    On Your Posts
  • Best Of All, It's Free!
  • Students Click Here

*Eng-Tips's functionality depends on members receiving e-mail. By joining you are opting in to receive e-mail.

Posting Guidelines

Promoting, selling, recruiting, coursework and thesis posting is forbidden.

Students Click Here

Jobs

ASME BPVC Code Case 2286-4 renamed in 2286-5

ASME BPVC Code Case 2286-4 renamed in 2286-5

ASME BPVC Code Case 2286-4 renamed in 2286-5

(OP)
Dear all,
I noticed Code Case 2286-4 is now renamed 2286-5 but can't find anything about this update in the Summary of Changes of ASME BPVC 2015; can anybody tell if there are major differences or the number was changed from -4 to -5 only because minor fixes and typos?

Best regards,
mb

RE: ASME BPVC Code Case 2286-4 renamed in 2286-5

The change to revision 5 was to revise below

The change of value of 1.147 to 1.2 of 4.4.12 (b) of Div.2 has been proposed by 15-96. Therefore 3.2.2 of CC2286-5 is also proposed for consistency because other sections use 1.2.

Red Flag This Post

Please let us know here why this post is inappropriate. Reasons such as off-topic, duplicates, flames, illegal, vulgar, or students posting their homework.

Red Flag Submitted

Thank you for helping keep Eng-Tips Forums free from inappropriate posts.
The Eng-Tips staff will check this out and take appropriate action.

Reply To This Thread

Posting in the Eng-Tips forums is a member-only feature.

Click Here to join Eng-Tips and talk with other members!


Resources