INTELLIGENT WORK FORUMS
FOR ENGINEERING PROFESSIONALS

Log In

Come Join Us!

Are you an
Engineering professional?
Join Eng-Tips Forums!
  • Talk With Other Members
  • Be Notified Of Responses
    To Your Posts
  • Keyword Search
  • One-Click Access To Your
    Favorite Forums
  • Automated Signatures
    On Your Posts
  • Best Of All, It's Free!
  • Students Click Here

*Eng-Tips's functionality depends on members receiving e-mail. By joining you are opting in to receive e-mail.

Posting Guidelines

Promoting, selling, recruiting, coursework and thesis posting is forbidden.

Students Click Here

Jobs

Ammonia Sphere Supporting Columns (Legs) Inspection.

Ammonia Sphere Supporting Columns (Legs) Inspection.

Ammonia Sphere Supporting Columns (Legs) Inspection.

(OP)
Hi,

We're operating two ammonia storage spheres for the last 35 years. The support columns (legs) of the spheres are protected against fire damage by means of concrete fireproofing, approx. 4-5 inches thick. The support columns are basically 32 in. pipes with 15 mm wall thickness. Can anyone share their experience for inspection of the support columns underneath the concrete fireproof coating.

Regards,

Red Flag This Post

Please let us know here why this post is inappropriate. Reasons such as off-topic, duplicates, flames, illegal, vulgar, or students posting their homework.

Red Flag Submitted

Thank you for helping keep Eng-Tips Forums free from inappropriate posts.
The Eng-Tips staff will check this out and take appropriate action.

Reply To This Thread

Posting in the Eng-Tips forums is a member-only feature.

Click Here to join Eng-Tips and talk with other members!


Resources