INTELLIGENT WORK FORUMS
FOR ENGINEERING PROFESSIONALS

Log In

Come Join Us!

Are you an
Engineering professional?
Join Eng-Tips Forums!
  • Talk With Other Members
  • Be Notified Of Responses
    To Your Posts
  • Keyword Search
  • One-Click Access To Your
    Favorite Forums
  • Automated Signatures
    On Your Posts
  • Best Of All, It's Free!
  • Students Click Here

*Eng-Tips's functionality depends on members receiving e-mail. By joining you are opting in to receive e-mail.

Posting Guidelines

Promoting, selling, recruiting, coursework and thesis posting is forbidden.

Students Click Here

Jobs

alcium chloride as a coagulant in rubber latex compound dip instead of calcium nitrate

alcium chloride as a coagulant in rubber latex compound dip instead of calcium nitrate

alcium chloride as a coagulant in rubber latex compound dip instead of calcium nitrate

(OP)
Can we use Calcium chloride as a coagulant in rubber latex compound dip instead of calcium nitrate ? Are there any negative effect for the final product or production lines.
Thank you

RE: alcium chloride as a coagulant in rubber latex compound dip instead of calcium nitrate

No personal experience but I know calcium chloride has been used in coagulant dipping. My worry is that it can be corrosive to ferrous metals including stainless steel. That may put some manufacturers off.

Red Flag This Post

Please let us know here why this post is inappropriate. Reasons such as off-topic, duplicates, flames, illegal, vulgar, or students posting their homework.

Red Flag Submitted

Thank you for helping keep Eng-Tips Forums free from inappropriate posts.
The Eng-Tips staff will check this out and take appropriate action.

Reply To This Thread

Posting in the Eng-Tips forums is a member-only feature.

Click Here to join Eng-Tips and talk with other members!


Resources