INTELLIGENT WORK FORUMS
FOR ENGINEERING PROFESSIONALS

Log In

Come Join Us!

Are you an
Engineering professional?
Join Eng-Tips Forums!
  • Talk With Other Members
  • Be Notified Of Responses
    To Your Posts
  • Keyword Search
  • One-Click Access To Your
    Favorite Forums
  • Automated Signatures
    On Your Posts
  • Best Of All, It's Free!
  • Students Click Here

*Eng-Tips's functionality depends on members receiving e-mail. By joining you are opting in to receive e-mail.

Posting Guidelines

Promoting, selling, recruiting, coursework and thesis posting is forbidden.

Students Click Here

Jobs

Stainless steel books

Stainless steel books

Stainless steel books

(OP)
Can anyone recommend good books for the design of Stainless Steel(particularly 304L/316L) - Annealing, pickling , passivating, service material requirements ( i.e. NACE MR0175) , hydro test ( max chlorides),
proper bolting selection, paint, etc.

Thanks

RE: Stainless steel books

Lippold and Kotecki, which has proven to be very useful for me (as a welding engineer), but this one doesn't really covers design. Still, it's a handy reference.

RE: Stainless steel books

Metals handbook Vol 5: Surface cleaning, finishing, and coating ...

Design for RELIABILITY, manufacturability, and maintainability

RE: Stainless steel books

There is also and ASM Stainless Steel handbook, it is a very succinct volume.
304 and 316 have very low tolerance to Cl, especially if you cannot force dry the system.
For hydro water we use 1ppm max Cl and 4 uSe conductivity.

= = = = = = = = = = = = = = = = = = = =
P.E. Metallurgy, Plymouth Tube

Red Flag This Post

Please let us know here why this post is inappropriate. Reasons such as off-topic, duplicates, flames, illegal, vulgar, or students posting their homework.

Red Flag Submitted

Thank you for helping keep Eng-Tips Forums free from inappropriate posts.
The Eng-Tips staff will check this out and take appropriate action.

Reply To This Thread

Posting in the Eng-Tips forums is a member-only feature.

Click Here to join Eng-Tips and talk with other members!


Resources