INTELLIGENT WORK FORUMS
FOR ENGINEERING PROFESSIONALS

Log In

Come Join Us!

Are you an
Engineering professional?
Join Eng-Tips Forums!
  • Talk With Other Members
  • Be Notified Of Responses
    To Your Posts
  • Keyword Search
  • One-Click Access To Your
    Favorite Forums
  • Automated Signatures
    On Your Posts
  • Best Of All, It's Free!
  • Students Click Here

*Eng-Tips's functionality depends on members receiving e-mail. By joining you are opting in to receive e-mail.

Posting Guidelines

Promoting, selling, recruiting, coursework and thesis posting is forbidden.

Students Click Here

Jobs

Aluminium Bus-bar welding

Aluminium Bus-bar welding

Aluminium Bus-bar welding

(OP)
Friends

Is the AWS D10.9 still exist. or any other standard supersede that.

RE: Aluminium Bus-bar welding

AWS D1.2 Structural Welding Code / Aluminum

Best regards - Al

RE: Aluminium Bus-bar welding

Most Buss Bar Manufacturers have their own requirements. Standard processes that we have used are GTAW and GMAW. Some require Qualification per ASME IX.

Red Flag This Post

Please let us know here why this post is inappropriate. Reasons such as off-topic, duplicates, flames, illegal, vulgar, or students posting their homework.

Red Flag Submitted

Thank you for helping keep Eng-Tips Forums free from inappropriate posts.
The Eng-Tips staff will check this out and take appropriate action.

Reply To This Thread

Posting in the Eng-Tips forums is a member-only feature.

Click Here to join Eng-Tips and talk with other members!


Resources