Low heat injection material
Low heat injection material
(OP)
Seeking a single component material requiring low heat (110 c) to become pliable, for low pressure injection of small flexible components.
The injection heat would initiate activation, creating a higher melt temperature (150 c+) once parts cool.
Similar to hot-glue being injected, but higher resistance to heat and more flexible (silicone, soft urethane consistency) after forming.
Thanks for any feedback
The injection heat would initiate activation, creating a higher melt temperature (150 c+) once parts cool.
Similar to hot-glue being injected, but higher resistance to heat and more flexible (silicone, soft urethane consistency) after forming.
Thanks for any feedback