INTELLIGENT WORK FORUMS
FOR ENGINEERING PROFESSIONALS

Log In

Come Join Us!

Are you an
Engineering professional?
Join Eng-Tips Forums!
  • Talk With Other Members
  • Be Notified Of Responses
    To Your Posts
  • Keyword Search
  • One-Click Access To Your
    Favorite Forums
  • Automated Signatures
    On Your Posts
  • Best Of All, It's Free!
  • Students Click Here

*Eng-Tips's functionality depends on members receiving e-mail. By joining you are opting in to receive e-mail.

Posting Guidelines

Promoting, selling, recruiting, coursework and thesis posting is forbidden.

Students Click Here

Jobs

Max Presuure in Brazed Copper Piping

Max Presuure in Brazed Copper Piping

Max Presuure in Brazed Copper Piping

(OP)
Hi All,

Please let me know that the maximum pressure that a brazed copper piping of size 1 1/4" can withstand.

Thanks in advance

RE: Max Presuure in Brazed Copper Piping

This is a vague question.
Pipe thickness?
Type of brazing alloy?
Length of brazing?
Type of copper alloy?
The code or spec it needs to meet?
All of these questions and more will dictate the strength of the pipe. Usually, the brazed area need to be calculated and designed such that it will be stronger than the bare pipe. Therefore, when a brazed pipe is tested till burst, it should burst along the bare pipe and never in the brazed area.

Red Flag This Post

Please let us know here why this post is inappropriate. Reasons such as off-topic, duplicates, flames, illegal, vulgar, or students posting their homework.

Red Flag Submitted

Thank you for helping keep Eng-Tips Forums free from inappropriate posts.
The Eng-Tips staff will check this out and take appropriate action.

Reply To This Thread

Posting in the Eng-Tips forums is a member-only feature.

Click Here to join Eng-Tips and talk with other members!


Resources