ALTERNATE MATERIAL REQUIREMENT FOR A234 WP11
ALTERNATE MATERIAL REQUIREMENT FOR A234 WP11
(OP)
Good Day Everybody,
Due to non-availability of material, required alternate material equivalent to 14" NPS A234 WP11 SCH 120 TEE.
Thanks in advance.
KAL
Due to non-availability of material, required alternate material equivalent to 14" NPS A234 WP11 SCH 120 TEE.
Thanks in advance.
KAL





RE: ALTERNATE MATERIAL REQUIREMENT FOR A234 WP11
Is the material a problem, or is it actually the Sch 120 thickness that you can't find.
RE: ALTERNATE MATERIAL REQUIREMENT FOR A234 WP11
RE: ALTERNATE MATERIAL REQUIREMENT FOR A234 WP11
RE: ALTERNATE MATERIAL REQUIREMENT FOR A234 WP11
Good Day,
Thanks for your comments.
Service : Ultra High Pressure steam.
SCH 120 A234 WP11 is found as off spec. and not available presently.
Hence, planned to utilize WP12 SCH 80 on temporary basis till the proposed off spec. material arrival.
RE: ALTERNATE MATERIAL REQUIREMENT FOR A234 WP11
Otherwise quoted by a tee in sch-160 which is more commercial.