Temper Bead WPS
Temper Bead WPS
(OP)
Developing a temper bead WPS Question I have is QW-403.27 am I reading this correct that this clause over rules thickness limits stated in Table QW-451.2.
INTELLIGENT WORK FORUMS
FOR ENGINEERING PROFESSIONALS Come Join Us!Are you an
Engineering professional? Join Eng-Tips Forums!
*Eng-Tips's functionality depends on members receiving e-mail. By joining you are opting in to receive e-mail. Posting GuidelinesJobs |
|
RE: Temper Bead WPS
See below
QW-290.3 Variables for Temper Bead Welding Qualifications.
Table QW-290.4 lists the essential and nonessential
variables that apply when temper bead qualification is required. The column “Hardness Test Essential
Variables” shall apply, except that when the applicable
Construction Code or Design Specification specifies
acceptance based on impact testing, the column “Impact
Test Essential Variables” shall apply.