coating integrity at lap joint of roof
coating integrity at lap joint of roof
(OP)
Not being well experienced with Tanks, I am reaching out to find experiences with coating integrity of tank interiors at lap joints. It is an API-650 Tank, carbon steel contruction. We have received conflicting recommendations...
Thanks in advance.
Thanks in advance.





RE: coating integrity at lap joint of roof
What recommendations have you received, with what background?
RE: coating integrity at lap joint of roof
Possible contractor is expressing reservations, coating supplier has advised to coat for application. Not sure if this is just a contractor that does not want to take the time to prepare surfaces correctly or if this is an area indicative of having problems with coating adhesion.
RE: coating integrity at lap joint of roof