INTELLIGENT WORK FORUMS
FOR ENGINEERING PROFESSIONALS

Log In

Come Join Us!

Are you an
Engineering professional?
Join Eng-Tips Forums!
  • Talk With Other Members
  • Be Notified Of Responses
    To Your Posts
  • Keyword Search
  • One-Click Access To Your
    Favorite Forums
  • Automated Signatures
    On Your Posts
  • Best Of All, It's Free!
  • Students Click Here

*Eng-Tips's functionality depends on members receiving e-mail. By joining you are opting in to receive e-mail.

Posting Guidelines

Promoting, selling, recruiting, coursework and thesis posting is forbidden.

Students Click Here

Jobs

27 NiCRMoV 15-6 - Equivalent

27 NiCRMoV 15-6 - Equivalent

27 NiCRMoV 15-6 - Equivalent

(OP)
27 NiCrMoV 15-6

Y-760 Mpa
T-900 Mpa

Trying to find a NA equivalent, our history he closest I can find would be a 4330V MOD for the high Ni

Anyone worked with this before and offered or determined an equivalent I can actually offer & get from supplier?

RE: 27 NiCRMoV 15-6 - Equivalent

Lack of information regarding application. With that said and no further information provided look at ASTM A 471, Class 1-6, depending on strength level.

RE: 27 NiCRMoV 15-6 - Equivalent

Just wanted to add that ASTM A470 Grade C might also be appropriate if this is for a forged shaft/rotor rather than a disk/wheel. ATI Forged Products would be one possible supplier.

Red Flag This Post

Please let us know here why this post is inappropriate. Reasons such as off-topic, duplicates, flames, illegal, vulgar, or students posting their homework.

Red Flag Submitted

Thank you for helping keep Eng-Tips Forums free from inappropriate posts.
The Eng-Tips staff will check this out and take appropriate action.

Reply To This Thread

Posting in the Eng-Tips forums is a member-only feature.

Click Here to join Eng-Tips and talk with other members!


Resources