the allowable operating temperature for a design life of ASTM A335 P11 pipes
the allowable operating temperature for a design life of ASTM A335 P11 pipes
(OP)
WHAT IS THE ALLOWABLE OPERATING TEMPRATURE RANGE FOR ASTM A335 P11 PIPES? OPERATING SERVICE TEMPRATURE AND NORMAL OPERATING PRESSURE IS 500 C AND 5.0 bara AND DESIGN TEMPRATURE IS 515 C. THE SERVICE FLUID IS COKE.
IT IS MY UNDERSTANDING BASED ON ASME B31.3 TABLE K-1 THAT USING P11 ABOVE 700F(371C)IS PROHIBITED.
Any web-based references or "white papers" would be appreciated...
IT IS MY UNDERSTANDING BASED ON ASME B31.3 TABLE K-1 THAT USING P11 ABOVE 700F(371C)IS PROHIBITED.
Any web-based references or "white papers" would be appreciated...





RE: the allowable operating temperature for a design life of ASTM A335 P11 pipes
Table K-1 is the wrong table to be looking at.
Edit The above is based on ASME B31.3-2014.
RE: the allowable operating temperature for a design life of ASTM A335 P11 pipes
MJCronin
Sr. Process Engineer
RE: the allowable operating temperature for a design life of ASTM A335 P11 pipes