Name and grade of this particular steel
Name and grade of this particular steel
(OP)
1) carbon (c) = 0.586
2) silicon (si) = 0.2658
3) manganese (Mn) = 0.607
4) phosphrous (P) = 0.0124
5) sulphur (S) = 0.0042
6) chromium (Cr) = 2.778
7) molybdenum ( Mo) = 0.0412
8) nickel (Ni) = 0.0943
9) alminium ( Al)= 0.0327
10) cobalt (Co) = 0.0082
11) copper (Cu) = 0.1951
12) neobium (Nb) = 0.0377
13) Titanium (Ti) = 0.0132
14) vinadium ( V) = 0.1391
15) tungsten (W) = 0.0125
16) lead (Pb) = 0.0234
17) Tin ( Sn) = 0.0158
18) magnesium ( Mg) = 0.0055
19) Boron (B) = 0.0013
20) Iron ( Fe) = 95.1
What is the grade and name of this steel?
2) silicon (si) = 0.2658
3) manganese (Mn) = 0.607
4) phosphrous (P) = 0.0124
5) sulphur (S) = 0.0042
6) chromium (Cr) = 2.778
7) molybdenum ( Mo) = 0.0412
8) nickel (Ni) = 0.0943
9) alminium ( Al)= 0.0327
10) cobalt (Co) = 0.0082
11) copper (Cu) = 0.1951
12) neobium (Nb) = 0.0377
13) Titanium (Ti) = 0.0132
14) vinadium ( V) = 0.1391
15) tungsten (W) = 0.0125
16) lead (Pb) = 0.0234
17) Tin ( Sn) = 0.0158
18) magnesium ( Mg) = 0.0055
19) Boron (B) = 0.0013
20) Iron ( Fe) = 95.1
What is the grade and name of this steel?





RE: Name and grade of this particular steel
Maybe 50B60.
I presume that you did the analysis by OE or XRF and that you have very good reference standards?
I say this because since yo listed all of them to 4 places you infer that you have that level of precision, which I don't believe. If this is off of a handheld device or EDS then you could be way off.
= = = = = = = = = = = = = = = = = = = =
P.E. Metallurgy, Plymouth Tube
RE: Name and grade of this particular steel
RE: Name and grade of this particular steel
RE: Name and grade of this particular steel
Your attachment shows a lab report hand written. This will never be accepted for any reference. Try using a better lab for your report.
"Even,if you are a minority of one, truth is the truth."
Mahatma Gandhi.
RE: Name and grade of this particular steel
If the V is real then maybe 6160, but then you wonder about the B.
The second one does not ring a bell with me.
= = = = = = = = = = = = = = = = = = = =
P.E. Metallurgy, Plymouth Tube