INTELLIGENT WORK FORUMS
FOR ENGINEERING PROFESSIONALS

Log In

Come Join Us!

Are you an
Engineering professional?
Join Eng-Tips Forums!
  • Talk With Other Members
  • Be Notified Of Responses
    To Your Posts
  • Keyword Search
  • One-Click Access To Your
    Favorite Forums
  • Automated Signatures
    On Your Posts
  • Best Of All, It's Free!
  • Students Click Here

*Eng-Tips's functionality depends on members receiving e-mail. By joining you are opting in to receive e-mail.

Posting Guidelines

Promoting, selling, recruiting, coursework and thesis posting is forbidden.

Students Click Here

Jobs

AISC Steel Manual Table 4-9 what is the meaning of the dashed line?

AISC Steel Manual Table 4-9 what is the meaning of the dashed line?

AISC Steel Manual Table 4-9 what is the meaning of the dashed line?

(OP)
Looking at Table 4-9 of AISC Steel Manual 13 ed (page 4-136), what is the significance of the dashed line?

It is also in the 14th edtion on page 4-137.

NOT THE BOLD LINE; which is the unbraced length that exceeds KL/r < 200


"God grant me the serenity, to accept the things I cannot change, the courage to change the things I can, and the wisdom to know the difference" -Reinhold Niebuhr

RE: AISC Steel Manual Table 4-9 what is the meaning of the dashed line?

Look at the commentary for Table 4-8 (Page 4-7 through 4-8 in my 14th Edition). It has to do with number of intermediate connectors between the two angles.

Check out Eng-Tips Forum's Policies here:
FAQ731-376: Eng-Tips.com Forum Policies

RE: AISC Steel Manual Table 4-9 what is the meaning of the dashed line?

(OP)
thanks

"God grant me the serenity, to accept the things I cannot change, the courage to change the things I can, and the wisdom to know the difference" -Reinhold Niebuhr

Red Flag This Post

Please let us know here why this post is inappropriate. Reasons such as off-topic, duplicates, flames, illegal, vulgar, or students posting their homework.

Red Flag Submitted

Thank you for helping keep Eng-Tips Forums free from inappropriate posts.
The Eng-Tips staff will check this out and take appropriate action.

Reply To This Thread

Posting in the Eng-Tips forums is a member-only feature.

Click Here to join Eng-Tips and talk with other members!


Resources