INTELLIGENT WORK FORUMS
FOR ENGINEERING PROFESSIONALS

Log In

Come Join Us!

Are you an
Engineering professional?
Join Eng-Tips Forums!
  • Talk With Other Members
  • Be Notified Of Responses
    To Your Posts
  • Keyword Search
  • One-Click Access To Your
    Favorite Forums
  • Automated Signatures
    On Your Posts
  • Best Of All, It's Free!
  • Students Click Here

*Eng-Tips's functionality depends on members receiving e-mail. By joining you are opting in to receive e-mail.

Posting Guidelines

Promoting, selling, recruiting, coursework and thesis posting is forbidden.

Students Click Here

Jobs

UW-11(a)(2)

UW-11(a)(2)

UW-11(a)(2)

(OP)
Hello Everyone,

Is there any governing Thickness to consider full radiography when butt welding two different thickness together?? please find attached case where 36mm dishend(MOC SA 516 Gr 60) is butt welded(SF to Shell) to 32 mm shell(MOC SA 516 Gr 60). AS per table UCS-57 p.no 1 if the thinner plate at welded joint exceed 32 than full radiography is mandatory. So in this case PV Elite result with mandatory full RT, while Codeware compress result in no radiography required.
so what is governing thickness for considering radiography requirement??

UW-11(a)(2) mention about nominal thickness of 38mm. Does it mean nominal thickness of 38mm is only for exclusive p.no & group than UCS-57???

Thanks.

RE: UW-11(a)(2)

Hi c8829,

Nominal thickness to be considered for determining Radiography requirement is defined in Code para UW-11(g).
I have reproduced the Code paragraph hereunder :

Quote (For radiographic and ultrasonic examination of butt welds, the definition of nominal thickness at the welded
joint under consideration shall be the nominal thickness of the thinner of the two parts joined. Nominal thickness
is defined in 3-2.)


So, for your case, the nominal thickness is 32mm.
As per UCS-57, nominal thickness above 32mm shall mandatorily require full radiography.However, for the case under consideration, nominal thickness does not exceed 32mm. Hence, Full RT is not mandatory.

RE: UW-11(a)(2)

(OP)
Thanks a lot chevproe. :)

RE: UW-11(a)(2)

Use software only for calculation, not for NDT
Regards
r6155

Red Flag This Post

Please let us know here why this post is inappropriate. Reasons such as off-topic, duplicates, flames, illegal, vulgar, or students posting their homework.

Red Flag Submitted

Thank you for helping keep Eng-Tips Forums free from inappropriate posts.
The Eng-Tips staff will check this out and take appropriate action.

Reply To This Thread

Posting in the Eng-Tips forums is a member-only feature.

Click Here to join Eng-Tips and talk with other members!


Resources