sa213 super 304H welding
sa213 super 304H welding
(OP)
We are looking at a project that involves welding of super alloy 304H. I am having issues finding any information on the the material at all much less what to weld it with. 2015 ASME Sec. IX list a UNS # S30432 that has the appropriate chemical composition of 18Cr 9Ni 3Cu Cb N (at least that is what I'm finding online, and in other post on this site). Does anyone have any information on welding this material?
Thanks,
Thanks,
powerplantcwi





RE: sa213 super 304H welding
http://www.tubular.nssmc.com/product-services/spec...
RE: sa213 super 304H welding
RE: sa213 super 304H welding