INTELLIGENT WORK FORUMS
FOR ENGINEERING PROFESSIONALS

Log In

Come Join Us!

Are you an
Engineering professional?
Join Eng-Tips Forums!
  • Talk With Other Members
  • Be Notified Of Responses
    To Your Posts
  • Keyword Search
  • One-Click Access To Your
    Favorite Forums
  • Automated Signatures
    On Your Posts
  • Best Of All, It's Free!
  • Students Click Here

*Eng-Tips's functionality depends on members receiving e-mail. By joining you are opting in to receive e-mail.

Posting Guidelines

Promoting, selling, recruiting, coursework and thesis posting is forbidden.

Students Click Here

Jobs

SA-249 N08367 stress values

SA-249 N08367 stress values

SA-249 N08367 stress values

(OP)
Experts,

I cannot find stress values for SA-249 UNS N08367 in Section II Part D.

Am I just overlooking them or are they really not there?

I have found them for SB-676 UNS N08367.

Thanks in advance,
numberfive

RE: SA-249 N08367 stress values

There is no stress line for N08367 under SA 249.

RE: SA-249 N08367 stress values

(OP)
Thanks

RE: SA-249 N08367 stress values

This is an odball material that is classified as ferrous in some specs and non-ferrous in others.

So although SA-249 N08367 may be commercially available, you must use SB-676 (for example) for Sec VIII, Div 1.

Regards,

Mike

The problem with sloppy work is that the supply FAR EXCEEDS the demand

RE: SA-249 N08367 stress values

(OP)
SnTMan,

This is exactly what we have found.

The customer supplied tubes (for use in a Sec. VIII, Div. 1 vessel repair) are marked and supplied with an MTR as being dual rated SA-249 / SB-676 N08367.

We will proceed and document as SB-676.

Thanks,
numberfive

RE: SA-249 N08367 stress values

numberfive, if certified to SB-676, you're good to go...

Regards,

Mike

The problem with sloppy work is that the supply FAR EXCEEDS the demand

Red Flag This Post

Please let us know here why this post is inappropriate. Reasons such as off-topic, duplicates, flames, illegal, vulgar, or students posting their homework.

Red Flag Submitted

Thank you for helping keep Eng-Tips Forums free from inappropriate posts.
The Eng-Tips staff will check this out and take appropriate action.

Reply To This Thread

Posting in the Eng-Tips forums is a member-only feature.

Click Here to join Eng-Tips and talk with other members!


Resources