Basic allowable stress for ASTM A 928 UNS S32750
Basic allowable stress for ASTM A 928 UNS S32750
(OP)
Hi all,
I'm developing wall thickness calculation for 18" ASTM A 928 UNS S32750 pipe, but I can't find basic allowable stress for this material in ASME B31.3. Is it possible to use the ASTM A 790 basic allowable stress value for A 928? Please kindly advise.
Regards.
I'm developing wall thickness calculation for 18" ASTM A 928 UNS S32750 pipe, but I can't find basic allowable stress for this material in ASME B31.3. Is it possible to use the ASTM A 790 basic allowable stress value for A 928? Please kindly advise.
Regards.





RE: Basic allowable stress for ASTM A 928 UNS S32750
I would do this ie. revert to ASTM A790 S32750 as basic allowable stress is stated in ASME B31.3 and also covers the welding type in ASTM A928 ie reference table A-1B EFW factor 1.0 when 100% X-ray.