INTELLIGENT WORK FORUMS
FOR ENGINEERING PROFESSIONALS

Log In

Come Join Us!

Are you an
Engineering professional?
Join Eng-Tips Forums!
  • Talk With Other Members
  • Be Notified Of Responses
    To Your Posts
  • Keyword Search
  • One-Click Access To Your
    Favorite Forums
  • Automated Signatures
    On Your Posts
  • Best Of All, It's Free!
  • Students Click Here

*Eng-Tips's functionality depends on members receiving e-mail. By joining you are opting in to receive e-mail.

Posting Guidelines

Promoting, selling, recruiting, coursework and thesis posting is forbidden.

Students Click Here

Jobs

ASME sec IX WPQT

ASME sec IX WPQT

ASME sec IX WPQT

(OP)
Dear All,
My Question is : If a welder has done performance qualification for SMAW using E-7018, would also qualified for E8018 ?
Note : other variables are unchanged

RE: ASME sec IX WPQT

Yes, assuming no other change from E7018 to E8018 (see ASME BPV Section IX Table QW 353), and as qualified with/without backing.

See ASME BPV Section IX, QW 404.15,and Tables QW-432 and QW-433.

RE: ASME sec IX WPQT

First, please review Section IX, QW-353, now look at filler metals, either a change in F-No or thickness deposited are essential variables. You can figure this out.

RE: ASME sec IX WPQT

For both electrodes the type of covering is Low-hydrogen potassium, iron powder (Designator 8). Electrodes with this covering type are assigned to F-No. 4 (see Tables QW-432).
Acc. to Table QW-353 with reference to QW-404.15 your welder is also qualified for E8018.

Regards - Juergen

Red Flag This Post

Please let us know here why this post is inappropriate. Reasons such as off-topic, duplicates, flames, illegal, vulgar, or students posting their homework.

Red Flag Submitted

Thank you for helping keep Eng-Tips Forums free from inappropriate posts.
The Eng-Tips staff will check this out and take appropriate action.

Reply To This Thread

Posting in the Eng-Tips forums is a member-only feature.

Click Here to join Eng-Tips and talk with other members!


Resources