INTELLIGENT WORK FORUMS
FOR ENGINEERING PROFESSIONALS

Log In

Come Join Us!

Are you an
Engineering professional?
Join Eng-Tips Forums!
  • Talk With Other Members
  • Be Notified Of Responses
    To Your Posts
  • Keyword Search
  • One-Click Access To Your
    Favorite Forums
  • Automated Signatures
    On Your Posts
  • Best Of All, It's Free!
  • Students Click Here

*Eng-Tips's functionality depends on members receiving e-mail. By joining you are opting in to receive e-mail.

Posting Guidelines

Promoting, selling, recruiting, coursework and thesis posting is forbidden.

Students Click Here

Jobs

QW-404.33

QW-404.33

QW-404.33

(OP)
i am not understanding QW-404.33. can some one elaborate it with simple examples???
QW-404.33
A change in the filler metal classification within an SFA specification, or, if not conforming to a filler metal classification within an SFA specification, a change in the manufacturer’s trade name for the filler metal. When optional supplemental designators, such as those
which indicate moisture resistance (i.e., XXXXR), diffusible hydrogen (i.e., XXXX H16, H8, etc.), and supplemental impact testing (i.e., XXXX‐1 or EXXXXM), are specified on the WPS, only filler metals which conform to the classification with the optional supplemental designator(s) specified on the WPS shall be used

RE: QW-404.33

Again, the designation i.e., are examples provided. What more do you need?

RE: QW-404.33

Examples:
A change from E7018 to E7016 or E7018-H4.
A change from E7018 H16 to E7018 H4.

RE: QW-404.33

(OP)
1-As per its 1st sentence, We can change 7018 with 7016 or any other Electrode of SFA 5.1 (if it fulfill other requirements e.g F #)
2-As per its 2nd Sentence, if Electrode is not enlisted in SFA then: I used electrode of company XYZ now can i change with electrode of company ABC while impact is not involved in WPS.
3- 3rd sentence is OK

RE: QW-404.33

For SMAW QW-404.33 is a non essential variable.

Red Flag This Post

Please let us know here why this post is inappropriate. Reasons such as off-topic, duplicates, flames, illegal, vulgar, or students posting their homework.

Red Flag Submitted

Thank you for helping keep Eng-Tips Forums free from inappropriate posts.
The Eng-Tips staff will check this out and take appropriate action.

Reply To This Thread

Posting in the Eng-Tips forums is a member-only feature.

Click Here to join Eng-Tips and talk with other members!


Resources