INTELLIGENT WORK FORUMS
FOR ENGINEERING PROFESSIONALS

Log In

Come Join Us!

Are you an
Engineering professional?
Join Eng-Tips Forums!
  • Talk With Other Members
  • Be Notified Of Responses
    To Your Posts
  • Keyword Search
  • One-Click Access To Your
    Favorite Forums
  • Automated Signatures
    On Your Posts
  • Best Of All, It's Free!
  • Students Click Here

*Eng-Tips's functionality depends on members receiving e-mail. By joining you are opting in to receive e-mail.

Posting Guidelines

Promoting, selling, recruiting, coursework and thesis posting is forbidden.

Students Click Here

Jobs

Need times for "hand finishing" stainless

Need times for "hand finishing" stainless

Need times for "hand finishing" stainless

(OP)
I am developing a spreadsheet for cost estimating custom built, stainless steel tanks.
Can anyone help with average times per unit area (or point me in the right direction) for finishing to 0.3Ra microns (240 grit) and to 0.1Ra (320 grit) from say No.1 Mill Finish 304 or 316 plate. A typical area would be say 10 sq.mtrs.
I understand that 1.25hrs/sq.mtr. is about industry average for 180 grit but that the resultant finish can vary from 0.3Ra to 0.8Ra and 15-17hrs/sq.mtr. for a mirror finish.
Any help at all, including comment re the 180 grit and mirror times I have, will be greatly appreciated and acknowledged.
Thanks

Red Flag This Post

Please let us know here why this post is inappropriate. Reasons such as off-topic, duplicates, flames, illegal, vulgar, or students posting their homework.

Red Flag Submitted

Thank you for helping keep Eng-Tips Forums free from inappropriate posts.
The Eng-Tips staff will check this out and take appropriate action.

Reply To This Thread

Posting in the Eng-Tips forums is a member-only feature.

Click Here to join Eng-Tips and talk with other members!


Resources