Impact testing dissimilar metals requirements ASME VIII Div 1
Impact testing dissimilar metals requirements ASME VIII Div 1
(OP)
Scenario:
Shell and tube HX (specific question is regarding the Shell to Tubesheet weld)
Shell side MDMT: -50 *F
Tube Side MDMT: -110*F
Shell material: SA-516-70N
Tubesheet material: SA-240-304
According to UCS-66 and UHA-51 all materials in question are exempt from impact testing, however UCS-67(a)(3) states that the weld wire must be impact tested.
Question:
Now since we are joining P1 to P8 we are using ER309L weld wire (which has a minimum temperature < -50*F), do we still have to purchase impact tested weld wire or qualify an impact tested PQR?
Thanks for any help, and if at all possible references would be most helpful
Shell and tube HX (specific question is regarding the Shell to Tubesheet weld)
Shell side MDMT: -50 *F
Tube Side MDMT: -110*F
Shell material: SA-516-70N
Tubesheet material: SA-240-304
According to UCS-66 and UHA-51 all materials in question are exempt from impact testing, however UCS-67(a)(3) states that the weld wire must be impact tested.
Question:
Now since we are joining P1 to P8 we are using ER309L weld wire (which has a minimum temperature < -50*F), do we still have to purchase impact tested weld wire or qualify an impact tested PQR?
Thanks for any help, and if at all possible references would be most helpful





RE: Impact testing dissimilar metals requirements ASME VIII Div 1