I had a quick question on SA-312 304L impact test requirements per b31.3. on EFW pipe since there is not filler material deposited to weld the joint does the pipe have to come impact tested at -320 per table 323.2.2 A-4(b)? The hardest part for me is getting over where it says "weld metal deposits" in A-4(b)and defining "deposits". Thanks in advance.
Christian
I had a quick question on SA-312 304L impact test requirements per b31.3. on EFW pipe since there is not filler material deposited to weld the joint does the pipe have to come impact tested at -320 per table 323.2.2 A-4(b)? The hardest part for me is getting over where it says "weld metal deposits" in A-4(b)and defining "deposits". Thanks in advance.
Christian