INTELLIGENT WORK FORUMS
FOR ENGINEERING PROFESSIONALS

Log In

Come Join Us!

Are you an
Engineering professional?
Join Eng-Tips Forums!
  • Talk With Other Members
  • Be Notified Of Responses
    To Your Posts
  • Keyword Search
  • One-Click Access To Your
    Favorite Forums
  • Automated Signatures
    On Your Posts
  • Best Of All, It's Free!
  • Students Click Here

*Eng-Tips's functionality depends on members receiving e-mail. By joining you are opting in to receive e-mail.

Posting Guidelines

Promoting, selling, recruiting, coursework and thesis posting is forbidden.

Students Click Here

Jobs

Anchors with welded plates

Anchors with welded plates

Anchors with welded plates

(OP)
An engineer came through the company for a few months and he exclaimed (rather emotionally) that the welded plates on the anchor heads cause lateral cracking in the concrete. There are some plant specifications from the 80's my new superior wants to use with this anchor type. Do you guys have the same opinion? Is there a study that concluded this finding?

RE: Anchors with welded plates

Section 5.5.3 of the attached document seems to support it. Section 5.5.4 states that if a termination plate is used, it should be small and circular. Keep in the mind the document was written for reciprocating compressors, but I imagine it's useful for most dynamic equipment.

Red Flag This Post

Please let us know here why this post is inappropriate. Reasons such as off-topic, duplicates, flames, illegal, vulgar, or students posting their homework.

Red Flag Submitted

Thank you for helping keep Eng-Tips Forums free from inappropriate posts.
The Eng-Tips staff will check this out and take appropriate action.

Reply To This Thread

Posting in the Eng-Tips forums is a member-only feature.

Click Here to join Eng-Tips and talk with other members!


Resources