INTELLIGENT WORK FORUMS
FOR ENGINEERING PROFESSIONALS

Log In

Come Join Us!

Are you an
Engineering professional?
Join Eng-Tips Forums!
  • Talk With Other Members
  • Be Notified Of Responses
    To Your Posts
  • Keyword Search
  • One-Click Access To Your
    Favorite Forums
  • Automated Signatures
    On Your Posts
  • Best Of All, It's Free!
  • Students Click Here

*Eng-Tips's functionality depends on members receiving e-mail. By joining you are opting in to receive e-mail.

Posting Guidelines

Promoting, selling, recruiting, coursework and thesis posting is forbidden.

Students Click Here

Jobs

Re-Tension a Post Tensioned Threaded Rod

Re-Tension a Post Tensioned Threaded Rod

Re-Tension a Post Tensioned Threaded Rod

(OP)
My company is currently constructing a wind farm next to one of our existing wind farms. My question is about the foundation anchor rods. The rods are typically #11 Grade 150 threaded rods (different turbine types may use different sized bolts such as #10, but that is not related to my question).

Typically, the anchor rods are post-tensioned, then 10% of the bolts are checked after initial torque, 10% of the bolts are tested again after the turbines operate for 500 hours, and 10% of the bolts are checked again after 1 year of operation. At our existing wind farm, the design engineers have signed off stating that no further testing is required. This is not typical as the engineers at our new wind farm are taking the more common approach of having 10% of the bolts being checked every other year for the life of the plant.

I am curious as to why the engineers at the first wind farm have decided that the bolts do not need to be tested throughout the life of the project, but the others require bi-annual testing? I am a young engineer and will not be making the decision on when rods should be tested, but some day I hope to get to that point in my career. The two issues I can think of which could require re-tensioning are relaxation of the post-tensioned rods and "rattling" loose of the bolts due to turbine vibration. Are these the two major factors requiring re-tensioning of a post-tensioned rod? Am I missing anything?

Thanks!

Red Flag This Post

Please let us know here why this post is inappropriate. Reasons such as off-topic, duplicates, flames, illegal, vulgar, or students posting their homework.

Red Flag Submitted

Thank you for helping keep Eng-Tips Forums free from inappropriate posts.
The Eng-Tips staff will check this out and take appropriate action.

Reply To This Thread

Posting in the Eng-Tips forums is a member-only feature.

Click Here to join Eng-Tips and talk with other members!


Resources