INTELLIGENT WORK FORUMS
FOR ENGINEERING PROFESSIONALS

Log In

Come Join Us!

Are you an
Engineering professional?
Join Eng-Tips Forums!
  • Talk With Other Members
  • Be Notified Of Responses
    To Your Posts
  • Keyword Search
  • One-Click Access To Your
    Favorite Forums
  • Automated Signatures
    On Your Posts
  • Best Of All, It's Free!
  • Students Click Here

*Eng-Tips's functionality depends on members receiving e-mail. By joining you are opting in to receive e-mail.

Posting Guidelines

Promoting, selling, recruiting, coursework and thesis posting is forbidden.

Students Click Here

Jobs

Crack initiation and propagation of Fibrous Composite in ANSYS

Crack initiation and propagation of Fibrous Composite in ANSYS

Crack initiation and propagation of Fibrous Composite in ANSYS

(OP)
Hi,

I am going to investigate the crack initiation and propagation transversely of fibrous composite in ANSYS. A quarter RVE with fibre and matrix is modelled and defined the cohesive element properties are defined by using command below:
tb,czm,3,,,expo
tbdata,1,tnmax,gmax,1000

After that, I have merge the layer between two elements. However, I am unable to mesh the cohesive zone layer with command below:
czmesh,,,1,x,0

An error was popped out "No cohesive has been created..." . I can't figure out any problem of it.

Can anyone tell me what is my problem or someone can give me alternative way to investigate the crack initiation and propagation of fibrous composite transversely.

Thank you

Red Flag This Post

Please let us know here why this post is inappropriate. Reasons such as off-topic, duplicates, flames, illegal, vulgar, or students posting their homework.

Red Flag Submitted

Thank you for helping keep Eng-Tips Forums free from inappropriate posts.
The Eng-Tips staff will check this out and take appropriate action.

Reply To This Thread

Posting in the Eng-Tips forums is a member-only feature.

Click Here to join Eng-Tips and talk with other members!


Resources