Nitric acid Pipe lines
Nitric acid Pipe lines
(OP)
why the designer select material for pipe will used for nitric acid as 304L with special containt NI > 9.5 % , why he didn't select 316L which include higher containt of NI ?
INTELLIGENT WORK FORUMS
FOR ENGINEERING PROFESSIONALS Come Join Us!Are you an
Engineering professional? Join Eng-Tips Forums!
*Eng-Tips's functionality depends on members receiving e-mail. By joining you are opting in to receive e-mail. Posting GuidelinesJobs |
|
RE: Nitric acid Pipe lines
http://www.nickelinstitute.org/~/Media/Files/Techn...
RE: Nitric acid Pipe lines
the temperature for the nitric acidd procees various between 122 °F to 290 °F .
nitric acid with 60% concentration fed to the nitric acid storage tank
RE: Nitric acid Pipe lines
RE: Nitric acid Pipe lines
RE: Nitric acid Pipe lines
RE: Nitric acid Pipe lines
I would be looking for special acid grade 310S for your application.
= = = = = = = = = = = = = = = = = = = =
P.E. Metallurgy, Plymouth Tube
RE: Nitric acid Pipe lines