ELBOW PSL2
ELBOW PSL2
(OP)
Good day:
As we turned PIPE 32 "-API 5L X60 PSL2, TO MAKE ELBOW OF 15°-20° This pipe LOSE THIS QUALITY PSL2 ?
THANK
JATE
As we turned PIPE 32 "-API 5L X60 PSL2, TO MAKE ELBOW OF 15°-20° This pipe LOSE THIS QUALITY PSL2 ?
THANK
JATE





RE: ELBOW PSL2
what radius?
Cold formed or hot formed?
If hot, how you heat up and cool down has a big impact on material properties, but the basic quality should be the same.
Remember - More details = better answers
Also: If you get a response it's polite to respond to it.
RE: ELBOW PSL2
(excuseme my bad english)
Thank