Weld Repair using different WPS
Weld Repair using different WPS
(OP)
Good Day,
I would like to ask if I can use a different WPS for weld repair as per ASME Sec IX QW-202.3 or QW-200.4?
Example:
WPS 1 (Original Weld)Process: GTAW+FCAW (BM Range= 5~38)
WPS 2 (Repair) Process: SMAW w/ back gouging (BM Range= 38 max)
No PWHT & Impact Test requirement
Thanks,
I would like to ask if I can use a different WPS for weld repair as per ASME Sec IX QW-202.3 or QW-200.4?
Example:
WPS 1 (Original Weld)Process: GTAW+FCAW (BM Range= 5~38)
WPS 2 (Repair) Process: SMAW w/ back gouging (BM Range= 38 max)
No PWHT & Impact Test requirement
Thanks,





RE: Weld Repair using different WPS
RE: Weld Repair using different WPS
Sir, thank you very much for your reply.