Wide Coil processed product tolerance
Wide Coil processed product tolerance
(OP)
Hi,
We received a SA240 Gr.316L coil product of 10 mm thickness. While referring Table A3.13 of SA480 Ed.2013 for thickness tolerance, we observed that maximum thickness given in the table is 8 mm. Then what will be the thickness tolerance for 10 mm coil. Whether the same for 8 mm is applicable for 10mm? Orelse whether i have to refere some other standard?
Guide us
BR,
M.V.Silambarasan
We received a SA240 Gr.316L coil product of 10 mm thickness. While referring Table A3.13 of SA480 Ed.2013 for thickness tolerance, we observed that maximum thickness given in the table is 8 mm. Then what will be the thickness tolerance for 10 mm coil. Whether the same for 8 mm is applicable for 10mm? Orelse whether i have to refere some other standard?
Guide us
BR,
M.V.Silambarasan