INTELLIGENT WORK FORUMS
FOR ENGINEERING PROFESSIONALS

Log In

Come Join Us!

Are you an
Engineering professional?
Join Eng-Tips Forums!
  • Talk With Other Members
  • Be Notified Of Responses
    To Your Posts
  • Keyword Search
  • One-Click Access To Your
    Favorite Forums
  • Automated Signatures
    On Your Posts
  • Best Of All, It's Free!
  • Students Click Here

*Eng-Tips's functionality depends on members receiving e-mail. By joining you are opting in to receive e-mail.

Posting Guidelines

Promoting, selling, recruiting, coursework and thesis posting is forbidden.

Students Click Here

Jobs

Fitness for Service - Brittle Fracture (Level 1 Assessment)

Fitness for Service - Brittle Fracture (Level 1 Assessment)

Fitness for Service - Brittle Fracture (Level 1 Assessment)

(OP)
Is level 1 assessment as per API 579 for brittle fracture applicable to P1 Group 1 & 2 materials only?
Just need this clarification to move forward.

Thank you.

Birken

RE: Fitness for Service - Brittle Fracture (Level 1 Assessment)

(OP)
Any thoughts over this one?

RE: Fitness for Service - Brittle Fracture (Level 1 Assessment)

See below right out of API 579

Carbon and low alloy could be P-No. 1 through P-No. 5A
3.1.1 This Part provides guidelines for evaluating the resistance to brittle fracture of existing carbon and low alloy steel pressure vessels, piping, and storage tanks. Other materials that could be susceptible to brittle fracture, such as ferritic, martensitic and duplex stainless steels, are not addressed in this Standard.

RE: Fitness for Service - Brittle Fracture (Level 1 Assessment)

(OP)
Thank you.
A mainstream FFS software created a doubt in my mind as it explicitly stated that Level-1 assessment is not applicable on materials other than P-No.1 G-No.1 & P-No.1 G-No.2.
Clear enough now, as Table 3.2 for Curves also mentions materials other than P-No.1 G-No.1 & P-No.1 G-No.2.

Red Flag This Post

Please let us know here why this post is inappropriate. Reasons such as off-topic, duplicates, flames, illegal, vulgar, or students posting their homework.

Red Flag Submitted

Thank you for helping keep Eng-Tips Forums free from inappropriate posts.
The Eng-Tips staff will check this out and take appropriate action.

Reply To This Thread

Posting in the Eng-Tips forums is a member-only feature.

Click Here to join Eng-Tips and talk with other members!


Resources