Coin edge on shim stock
Coin edge on shim stock
(OP)
We are having issues cutting 302SS .004" Shim stock. we are getting a dime edge. at this place they are using an old S48 CO2 Laser, does it in pulsed and CW and in different locations.
"I am stuck on Band-Aid brand, 'cause they are stuck on me"





RE: Coin edge on shim stock
I have seen material bouncing up and down relative to the nozzle causing the kerf to get wider and narrower with the distance from the focal point.
Just a though...
RE: Coin edge on shim stock
Chris Krug http://krugtech.com/
Maximum Up-time, Minimum BS
RE: Coin edge on shim stock
"I am stuck on Band-Aid brand, 'cause they are stuck on me"