INTELLIGENT WORK FORUMS
FOR ENGINEERING PROFESSIONALS

Log In

Come Join Us!

Are you an
Engineering professional?
Join Eng-Tips Forums!
  • Talk With Other Members
  • Be Notified Of Responses
    To Your Posts
  • Keyword Search
  • One-Click Access To Your
    Favorite Forums
  • Automated Signatures
    On Your Posts
  • Best Of All, It's Free!
  • Students Click Here

*Eng-Tips's functionality depends on members receiving e-mail. By joining you are opting in to receive e-mail.

Posting Guidelines

Promoting, selling, recruiting, coursework and thesis posting is forbidden.

Students Click Here

Jobs

Limiting Curvature in Pipe piles

Limiting Curvature in Pipe piles

Limiting Curvature in Pipe piles

(OP)
Does anyone know of a limiting curvature value for (driven)pipe piles?

RE: Limiting Curvature in Pipe piles

From

PCI
Standard Prestressed Concrete Piles
General Notes

"TOLERANCES
...
Accumulated deviation from straightmess measured along two perpendicular faces of the pile when not subject to bending shall not exceed 1/8 in. per 10 ft. of length. Note that long prestressed piles may be inherently flexible and excess sweep may be a temporary condition due to method of storage."

It seems to indicate that may be delivered to site with some out of straightedness due to storage. You would have to hang then vertically for some time and then measure the out of straightedness, or something like so seems to imply.

Red Flag This Post

Please let us know here why this post is inappropriate. Reasons such as off-topic, duplicates, flames, illegal, vulgar, or students posting their homework.

Red Flag Submitted

Thank you for helping keep Eng-Tips Forums free from inappropriate posts.
The Eng-Tips staff will check this out and take appropriate action.

Reply To This Thread

Posting in the Eng-Tips forums is a member-only feature.

Click Here to join Eng-Tips and talk with other members!


Resources