CS or maybe SS using
CS or maybe SS using
(OP)
The RSI value of RO permeate is specified from 11 to 15.8. This value means as “severe corrosion”.
Further to the review of RSI, unexpected corrosion product and scale particle may affect to the operation and maintenance of demineralization package. pls advice me whether carbon steel is appropriate or not. if not why?
Further to the review of RSI, unexpected corrosion product and scale particle may affect to the operation and maintenance of demineralization package. pls advice me whether carbon steel is appropriate or not. if not why?





RE: CS or maybe SS using
And by carbon steel, do you mean black pipe? Or seamless? Or welded? Need more info to help.
Bill Riehl
Riehl Engineering
RE: CS or maybe SS using
One option is to use Schedule 80 PVC piping & fittings. A second option is to use 316 stainless steel piping and fittings. A third option is FRP.
RE: CS or maybe SS using
= = = = = = = = = = = = = = = = = = = =
P.E. Metallurgy, Plymouth Tube