INTELLIGENT WORK FORUMS
FOR ENGINEERING PROFESSIONALS

Log In

Come Join Us!

Are you an
Engineering professional?
Join Eng-Tips Forums!
  • Talk With Other Members
  • Be Notified Of Responses
    To Your Posts
  • Keyword Search
  • One-Click Access To Your
    Favorite Forums
  • Automated Signatures
    On Your Posts
  • Best Of All, It's Free!
  • Students Click Here

*Eng-Tips's functionality depends on members receiving e-mail. By joining you are opting in to receive e-mail.

Posting Guidelines

Promoting, selling, recruiting, coursework and thesis posting is forbidden.

Students Click Here

Jobs

HCl and HF, in the same piping system

HCl and HF, in the same piping system

HCl and HF, in the same piping system

(OP)
In a piping system that will have 36% HCl ran through it and then purged with air and then 6% HF run through at ambient temperature, would you expect any issues using C276? Or possibly another alloy? I am thinking C276 just because its resistance to HCl but not so sure with the HF, I know it is not as resistant to HF but my concern is with any residual acid that is left over during the purge. Anybody have experience with a system where two different acids are ran through the same piping system.

Red Flag This Post

Please let us know here why this post is inappropriate. Reasons such as off-topic, duplicates, flames, illegal, vulgar, or students posting their homework.

Red Flag Submitted

Thank you for helping keep Eng-Tips Forums free from inappropriate posts.
The Eng-Tips staff will check this out and take appropriate action.