Advice for Weld Overlay in vessel required:
Advice for Weld Overlay in vessel required:
(OP)
one of the vessel we had the issue of preferential weld erosion corrosion as compared to parent metal (shell course/dished head), up to the height of ~3.5m from bottom dished head. It was repaired by welding.
Advice on suitability of weld overlaying of above specified affected area (say 3.5 to 4m height) by duplex /super duplex stainless steel (e.g. 2707 grade).
Advice on suitability of weld overlaying of above specified affected area (say 3.5 to 4m height) by duplex /super duplex stainless steel (e.g. 2707 grade).





RE: Advice for Weld Overlay in vessel required:
RE: Advice for Weld Overlay in vessel required:
Keeping the correct composition and microstructure with no secondary phases is very difficult.
This is why austenitic alloys are most commonly used for overlay.
= = = = = = = = = = = = = = = = = = = =