INTELLIGENT WORK FORUMS
FOR ENGINEERING PROFESSIONALS

Log In

Come Join Us!

Are you an
Engineering professional?
Join Eng-Tips Forums!
  • Talk With Other Members
  • Be Notified Of Responses
    To Your Posts
  • Keyword Search
  • One-Click Access To Your
    Favorite Forums
  • Automated Signatures
    On Your Posts
  • Best Of All, It's Free!
  • Students Click Here

*Eng-Tips's functionality depends on members receiving e-mail. By joining you are opting in to receive e-mail.

Posting Guidelines

Promoting, selling, recruiting, coursework and thesis posting is forbidden.

Students Click Here

Jobs

AISI 329 / 1.4460 STAINLESS STEEL

AISI 329 / 1.4460 STAINLESS STEEL

AISI 329 / 1.4460 STAINLESS STEEL

(OP)
Dear All,

Request to advise if AISI 329 or 1.4460 complies and can be certified as per NACE MR0175 or MR0103 Latest editions.

Please explain in details if possible.

Regards

thanks

RE: AISI 329 / 1.4460 STAINLESS STEEL

Duplex stainless steel type 329 would meet NACE MR0175/ISO 15156-3 if the molybdenum concentration is at least 1.5 %.

Red Flag This Post

Please let us know here why this post is inappropriate. Reasons such as off-topic, duplicates, flames, illegal, vulgar, or students posting their homework.

Red Flag Submitted

Thank you for helping keep Eng-Tips Forums free from inappropriate posts.
The Eng-Tips staff will check this out and take appropriate action.

Reply To This Thread

Posting in the Eng-Tips forums is a member-only feature.

Click Here to join Eng-Tips and talk with other members!


Resources