INTELLIGENT WORK FORUMS
FOR ENGINEERING PROFESSIONALS

Log In

Come Join Us!

Are you an
Engineering professional?
Join Eng-Tips Forums!
  • Talk With Other Members
  • Be Notified Of Responses
    To Your Posts
  • Keyword Search
  • One-Click Access To Your
    Favorite Forums
  • Automated Signatures
    On Your Posts
  • Best Of All, It's Free!
  • Students Click Here

*Eng-Tips's functionality depends on members receiving e-mail. By joining you are opting in to receive e-mail.

Posting Guidelines

Promoting, selling, recruiting, coursework and thesis posting is forbidden.

Students Click Here

Jobs

Heat transfer coefficients for neoprene rubber

Heat transfer coefficients for neoprene rubber

Heat transfer coefficients for neoprene rubber

(OP)
Hello all,

I'm looking for heat transfer coefficients for neoprene rubber (or any rubber in that case).

Mainly:

1. Conductivity
2. Emissivity
3. Specific Heat
4. Convection coefficient with air (not enclosed air)

Thank you very much! It is greatly appreciated! If the reference is provided it's going to be even more!

Thank you in advance!

RE: Heat transfer coefficients for neoprene rubber

For Cp and k

http://www.makeitfrom.com/compare/Chloroprene-Rubb...


For total emissivity, rubber - glossy finish at 74degF = 0.945 ( Perry Chem Engg Handbook, chapter on radiation, table 5-6, page 5-29)

Convection coeff should be calculated - pls look up any heat transfer textbook and read up on natural convection heat transfer)

RE: Heat transfer coefficients for neoprene rubber

Settler:

The ASHRAE Handbook of Fundamentals has those values in the material properties table.

Regards,

DB

RE: Heat transfer coefficients for neoprene rubber

(OP)
Thank you very much all of you!

Red Flag This Post

Please let us know here why this post is inappropriate. Reasons such as off-topic, duplicates, flames, illegal, vulgar, or students posting their homework.

Red Flag Submitted

Thank you for helping keep Eng-Tips Forums free from inappropriate posts.
The Eng-Tips staff will check this out and take appropriate action.

Reply To This Thread

Posting in the Eng-Tips forums is a member-only feature.

Click Here to join Eng-Tips and talk with other members!


Resources