welding pipe
welding pipe
(OP)
Hello all,
We have following two welding procedure to butt weld API X52 NPS20 X 12.4 mm pipe. My first option would be procedure#1; however, is there any issue welding with procedure#2? Thanks for your inputs.
#1 root E6010 hot, fill and cap E7010
#2 root E6010 hot E8010 fill and cap E8018
We have following two welding procedure to butt weld API X52 NPS20 X 12.4 mm pipe. My first option would be procedure#1; however, is there any issue welding with procedure#2? Thanks for your inputs.
#1 root E6010 hot, fill and cap E7010
#2 root E6010 hot E8010 fill and cap E8018