PSL1 AND PSL2
PSL1 AND PSL2
(OP)
Hello, i have a question:
If a material PSL1 is meeting the requirements of PSL2, is it acceptable to use it as PSL2 ?
i repeat a question that was not nobody answered ( 2 or 3 years before)
Thank for help me.
JATE
If a material PSL1 is meeting the requirements of PSL2, is it acceptable to use it as PSL2 ?
i repeat a question that was not nobody answered ( 2 or 3 years before)
Thank for help me.
JATE





RE: PSL1 AND PSL2
Other than the fact that PSL2 pipe is "better" and has a much higher traceability and testing, there is no physical difference and no design impact. However for selling it as PSL2, I don't think that is a practical proposition - far too many additional things need to have been done and recorded to make it happen in reality.
Remember - More details = better answers
Also: If you get a response it's polite to respond to it.
RE: PSL1 AND PSL2
RE: PSL1 AND PSL2
Nice try, but I wouldn't accept it if it was me.
Remember - More details = better answers
Also: If you get a response it's polite to respond to it.
RE: PSL1 AND PSL2
RE: PSL1 AND PSL2
Additional testing requirements under PSL-2 include CVN testing, non-destructive inspection of seamless products, certification to SR15, and mandatory traceability throughout the entire production process. Most FERC, DOT, or FEMSA lines require PSL-2, meaning these types of requirements are a must when supplying pipe for pipelines that are regulated by any of these governing bodies.
PSL-1 pipe will not meet the requirements of PSL2.
RE: PSL1 AND PSL2