INTELLIGENT WORK FORUMS
FOR ENGINEERING PROFESSIONALS

Log In

Come Join Us!

Are you an
Engineering professional?
Join Eng-Tips Forums!
  • Talk With Other Members
  • Be Notified Of Responses
    To Your Posts
  • Keyword Search
  • One-Click Access To Your
    Favorite Forums
  • Automated Signatures
    On Your Posts
  • Best Of All, It's Free!
  • Students Click Here

*Eng-Tips's functionality depends on members receiving e-mail. By joining you are opting in to receive e-mail.

Posting Guidelines

Promoting, selling, recruiting, coursework and thesis posting is forbidden.

Students Click Here

Jobs

Switchgear and Xylene?

Switchgear and Xylene?

Switchgear and Xylene?

(OP)
Have some folks who would like to use an acetone and xylene based degreaser as an all-purpose switchgear cleaner. Seeing what this stuff can do to plastic makes me believe this is a really bad idea, but I can't find much substantiation against it.

I know alcohol is the industry standard and can find a fair bit of support for that, but I could've sworn I'd seen OEM notes specifically prohibiting using xylene on some medium-voltage insulation.

Anyone familiar with literature to back that up?

RE: Switchgear and Xylene?

Maybe try with hexane, it's way less hard on plastics than acetone, but may have less cleaning power. Alcools (ex: methanol and rubbing alcool) and acetone, if not pure, will contain traces of water.

Red Flag This Post

Please let us know here why this post is inappropriate. Reasons such as off-topic, duplicates, flames, illegal, vulgar, or students posting their homework.

Red Flag Submitted

Thank you for helping keep Eng-Tips Forums free from inappropriate posts.
The Eng-Tips staff will check this out and take appropriate action.

Reply To This Thread

Posting in the Eng-Tips forums is a member-only feature.

Click Here to join Eng-Tips and talk with other members!


Resources