low alloy steel
low alloy steel
(OP)
Is ASME SA-516-70 Normalized material considered low alloy steel?
INTELLIGENT WORK FORUMS
FOR ENGINEERING PROFESSIONALS Come Join Us!Are you an
Engineering professional? Join Eng-Tips Forums!
*Eng-Tips's functionality depends on members receiving e-mail. By joining you are opting in to receive e-mail. Posting GuidelinesJobs |
|
RE: low alloy steel
RE: low alloy steel
Regards,
Mike
RE: low alloy steel
That is exactly why you stay out of metallurgical semantics. The chemical composition ranges for SA-516 meet the category for carbon steel plate. Now you start adding spices like V, Cb, and Ti, you start moving into high strength low-alloy steels or Cr and Mo spices, and you are into families of common low-alloy steels.
RE: low alloy steel
Etc, etc.
RE: low alloy steel